Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane
Mixed matrix membranes (MMMs) comprising polysulfone (PSF) Udel® P-1700 and 30 wt% carbon molecular sieve (CMS) particles (<25 μm) have been fabricated and characterized. CMS particles were treated in poly(vinyl pyrrolidone) kollidone 15 (PVP K-15) sizing bath solution (1–10 wt% in isopropano...
Saved in:
Main Authors: | , |
---|---|
Format: | Article |
Published: |
Elsevier B.V.
2008
|
Subjects: | |
Online Access: | http://eprints.utm.my/id/eprint/7215/ http://dx.doi.org/10.1016/j.memsci.2007.09.007 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.utm.7215 |
---|---|
record_format |
eprints |
spelling |
my.utm.72152017-10-22T08:41:03Z http://eprints.utm.my/id/eprint/7215/ Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane W. A. W., Rafizah Ismail, A. F. TP Chemical technology Mixed matrix membranes (MMMs) comprising polysulfone (PSF) Udel® P-1700 and 30 wt% carbon molecular sieve (CMS) particles (<25 μm) have been fabricated and characterized. CMS particles were treated in poly(vinyl pyrrolidone) kollidone 15 (PVP K-15) sizing bath solution (1–10 wt% in isopropanol) prior to embedment into the matrix solution to improve matrix–sieve interfacial adhesion. This study investigated the effects of CMS sizing with PVP K-15 on the morphology and the gas separation performance of PSF–CMS MMMs. The fabricated MMMs were characterized using TGA, DSC, FESEM, ATR-FTIR and single gas permeation test using high purity O2 and N2. A dramatic improvement in CMS–PSF adhesion was observed using FESEM micrographs upon incorporation of PVP K-15-sized CMS particles. ATR-FTIR results suggest the occurrence of intermolecular interaction between PVP K-15 sizing layer on the outer surface of CMS particles and PSF matrix. A substantial recovery of separation performance was achieved whereby the PSF–PVP-sized CMS MMM exhibited 1.7 times higher O2/N2 selectivity compared to that of unmodified MMM Elsevier B.V. 2008 Article PeerReviewed W. A. W., Rafizah and Ismail, A. F. (2008) Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane. Journal of Membrane Science, 307 . pp. 53-61. ISSN 0376-7388 http://dx.doi.org/10.1016/j.memsci.2007.09.007 10.1016/j.memsci.2007.09.007 |
institution |
Universiti Teknologi Malaysia |
building |
UTM Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Teknologi Malaysia |
content_source |
UTM Institutional Repository |
url_provider |
http://eprints.utm.my/ |
topic |
TP Chemical technology |
spellingShingle |
TP Chemical technology W. A. W., Rafizah Ismail, A. F. Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
description |
Mixed matrix membranes (MMMs) comprising polysulfone (PSF) Udel® P-1700 and 30 wt% carbon molecular sieve (CMS) particles (<25 μm) have been fabricated and characterized. CMS particles were treated in poly(vinyl pyrrolidone) kollidone 15 (PVP K-15) sizing bath solution (1–10 wt% in isopropanol) prior to embedment into the matrix solution to improve matrix–sieve interfacial adhesion. This study investigated the effects of CMS sizing with PVP K-15 on the morphology and the gas separation performance of PSF–CMS MMMs. The fabricated MMMs were characterized using TGA, DSC, FESEM, ATR-FTIR and single gas permeation test using high purity O2 and N2. A dramatic improvement in CMS–PSF adhesion was observed using FESEM micrographs upon incorporation of PVP K-15-sized CMS particles. ATR-FTIR results suggest the occurrence of intermolecular interaction between PVP K-15 sizing layer on the outer surface of CMS particles and PSF matrix. A substantial recovery of separation performance was achieved whereby the PSF–PVP-sized CMS MMM exhibited 1.7 times higher O2/N2 selectivity compared to that of unmodified MMM |
format |
Article |
author |
W. A. W., Rafizah Ismail, A. F. |
author_facet |
W. A. W., Rafizah Ismail, A. F. |
author_sort |
W. A. W., Rafizah |
title |
Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
title_short |
Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
title_full |
Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
title_fullStr |
Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
title_full_unstemmed |
Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
title_sort |
effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) k-15 on carbon molecular sieve–polysulfone mixed matrix membrane |
publisher |
Elsevier B.V. |
publishDate |
2008 |
url |
http://eprints.utm.my/id/eprint/7215/ http://dx.doi.org/10.1016/j.memsci.2007.09.007 |
_version_ |
1643644725037629440 |
score |
13.211869 |