Effect of carbon molecular sieve sizing with poly(vinyl pyrrolidone) K-15 on carbon molecular sieve–polysulfone mixed matrix membrane

Mixed matrix membranes (MMMs) comprising polysulfone (PSF) Udel® P-1700 and 30 wt% carbon molecular sieve (CMS) particles (<25 μm) have been fabricated and characterized. CMS particles were treated in poly(vinyl pyrrolidone) kollidone 15 (PVP K-15) sizing bath solution (1–10 wt% in isopropano...

Full description

Saved in:
Bibliographic Details
Main Authors: W. A. W., Rafizah, Ismail, A. F.
Format: Article
Published: Elsevier B.V. 2008
Subjects:
Online Access:http://eprints.utm.my/id/eprint/7215/
http://dx.doi.org/10.1016/j.memsci.2007.09.007