Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect
Thick film has demonstrated a high Seebeck coefficient, S, for thermoelectric material but it is very challenging to obtain through cost-effective techniques. Electrodeposition is adopted to tailor the film's thickness, t, facilitated by additive and heat treatment to boost the S. Here, we repo...
Saved in:
Main Authors: | , , , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
IOP Publishing Ltd
2021
|
Online Access: | http://eprints.utem.edu.my/id/eprint/25623/2/2021_2%20Q1%20ENHANCED%20THERNOELECTRIC%20PROPERTIES%20OF%20SKUTTERUDITE.PDF http://eprints.utem.edu.my/id/eprint/25623/ https://iopscience.iop.org/article/10.1149/1945-7111/ac13d0/pdf |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.utem.eprints.25623 |
---|---|
record_format |
eprints |
spelling |
my.utem.eprints.256232022-03-08T11:32:09Z http://eprints.utem.edu.my/id/eprint/25623/ Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect Mohd Sabri, Mohd Faizul Sabran, Nuur Syahidah Fadzallah, Iman Aris Ono, Takahito Samat, Khairul Fadzli Yusuf, Siti Nor Farhana Saidur, Rahman Thick film has demonstrated a high Seebeck coefficient, S, for thermoelectric material but it is very challenging to obtain through cost-effective techniques. Electrodeposition is adopted to tailor the film's thickness, t, facilitated by additive and heat treatment to boost the S. Here, we report the influence of two varied molecular weight (Mw) of polyvinyl alcohol (PVA) as additive and the post-deposition annealing temperature on Skuterrudite (cobalt triantimonide, CoSb3) thick films. The films are synthesized at room temperature via chronoamperometry from an aqueous electrolyte consisting of cobalt and antimony ions assisted with PVA (1800 and 98 000 Da). Higher Mw exhibits fine grains and uniform layers with the t of ∼13 μm in 2 h deposition time due to the greater ion diffusion coefficient, D (1.52 × 10-5 cm2s-1). The post-deposition annealing on the CoSb3 thick film of higher Mw PVA assisted revealed significant enhancement of the S and power factor, PF by over 100% as compared to the as-deposited film. Low electrical conductivity, σ of 7.53 kSm-1 contributes to the high S and PF (annealed at 373.15 K) of 222.75 μVK-1 and 558.17 μWm-1K-2, respectively. This work demonstrates that post-deposition annealing has a prominent effect on thermoelectric properties. IOP Publishing Ltd 2021-07 Article PeerReviewed text en http://eprints.utem.edu.my/id/eprint/25623/2/2021_2%20Q1%20ENHANCED%20THERNOELECTRIC%20PROPERTIES%20OF%20SKUTTERUDITE.PDF Mohd Sabri, Mohd Faizul and Sabran, Nuur Syahidah and Fadzallah, Iman Aris and Ono, Takahito and Samat, Khairul Fadzli and Yusuf, Siti Nor Farhana and Saidur, Rahman (2021) Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect. Journal of The Electrochemical Society, 168 (7). pp. 1-10. ISSN 0013-4651 https://iopscience.iop.org/article/10.1149/1945-7111/ac13d0/pdf 10.1149/1945-7111/ac13d0 |
institution |
Universiti Teknikal Malaysia Melaka |
building |
UTEM Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Teknikal Malaysia Melaka |
content_source |
UTEM Institutional Repository |
url_provider |
http://eprints.utem.edu.my/ |
language |
English |
description |
Thick film has demonstrated a high Seebeck coefficient, S, for thermoelectric material but it is very challenging to obtain through cost-effective techniques. Electrodeposition is adopted to tailor the film's thickness, t, facilitated by additive and heat treatment to boost the S. Here, we report the influence of two varied molecular weight (Mw) of polyvinyl alcohol (PVA) as additive and the post-deposition annealing temperature on Skuterrudite (cobalt triantimonide, CoSb3) thick films. The films are synthesized at room temperature via chronoamperometry from an aqueous electrolyte consisting of cobalt and antimony ions assisted with PVA (1800 and 98 000 Da). Higher Mw exhibits fine grains and uniform layers with the t of ∼13 μm in 2 h deposition time due to the greater ion diffusion coefficient, D (1.52 × 10-5 cm2s-1). The post-deposition annealing on the CoSb3 thick film of higher Mw PVA assisted revealed significant enhancement of the S and power factor, PF by over 100% as compared to the as-deposited film. Low electrical conductivity, σ of 7.53 kSm-1 contributes to the high S and PF (annealed at 373.15 K) of 222.75 μVK-1 and 558.17 μWm-1K-2, respectively. This work demonstrates that post-deposition annealing has a prominent effect on thermoelectric properties. |
format |
Article |
author |
Mohd Sabri, Mohd Faizul Sabran, Nuur Syahidah Fadzallah, Iman Aris Ono, Takahito Samat, Khairul Fadzli Yusuf, Siti Nor Farhana Saidur, Rahman |
spellingShingle |
Mohd Sabri, Mohd Faizul Sabran, Nuur Syahidah Fadzallah, Iman Aris Ono, Takahito Samat, Khairul Fadzli Yusuf, Siti Nor Farhana Saidur, Rahman Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect |
author_facet |
Mohd Sabri, Mohd Faizul Sabran, Nuur Syahidah Fadzallah, Iman Aris Ono, Takahito Samat, Khairul Fadzli Yusuf, Siti Nor Farhana Saidur, Rahman |
author_sort |
Mohd Sabri, Mohd Faizul |
title |
Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect |
title_short |
Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect |
title_full |
Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect |
title_fullStr |
Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect |
title_full_unstemmed |
Enhanced Thermoelectric Properties Of Skutterudite Thick Film Polyvinyl Alcohol Assisted From The Post-Deposition Annealing Effect |
title_sort |
enhanced thermoelectric properties of skutterudite thick film polyvinyl alcohol assisted from the post-deposition annealing effect |
publisher |
IOP Publishing Ltd |
publishDate |
2021 |
url |
http://eprints.utem.edu.my/id/eprint/25623/2/2021_2%20Q1%20ENHANCED%20THERNOELECTRIC%20PROPERTIES%20OF%20SKUTTERUDITE.PDF http://eprints.utem.edu.my/id/eprint/25623/ https://iopscience.iop.org/article/10.1149/1945-7111/ac13d0/pdf |
_version_ |
1726795998843371520 |
score |
13.211869 |