Effect Of High Temperature On Oxidation Behavior Of Superheater Materials Formation Of Protective Oxide Scale
The oxidation behaviour of Ni-based superalloy C22 and commercial steel 304 SS were investigated at high temperature 800, 900 and 1000˚C with exposure times 24 h under oxidized atmosphere (air). The microsturucture of C22 and 304 SS was characterized by scanning electron microscope (SEM). The compos...
Saved in:
Main Author: | Abdul Wahab, Haziq Mudzakir |
---|---|
Format: | Monograph |
Language: | English |
Published: |
Universiti Sains Malaysia
2018
|
Subjects: | |
Online Access: | http://eprints.usm.my/53034/1/Effect%20Of%20Fused%20Deposition%20Modelling%20Fabrication%20Parameters%20On%20The%20Tensile%20Properties%20Of%20Acrylonitrile%20Butadiene%20Styrene_Chua%20Jing%20Ting_B1_2018.pdf http://eprints.usm.my/53034/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Formation of protective Cr2O3 scale at high temperature and the effect of mass transport in the presence of water vapor
by: Ani, Mohd Hanafi, et al.
Published: (2012) -
Effect Of Nb, Cr And W On The High Temperature Oxidation
Behavior Of Ti-Al Alloys
by: Sapiai, Napisah
Published: (2011) -
Synthesis of iron oxide nanoflakes at lower temperature by air oxidation of iron foils
by: Mohamed Rashid, Norhana, et al.
Published: (2014) -
Effect Of Nitric-Oxide Post-Oxidation Annealing On High-Temperature Oxidized 4H SiC.
by: Jeong, Hyun Moon, et al.
Published: (2007) -
Formation of Nanotubular TiOa Bioactive
Oxide Layer on Titanium and Cell
Response Studies
by
by: Sreekantan, Srimala, et al.
Published: (2011)