Open-cell copper foam joining: joint strength and interfacial behaviour
A copper (Cu) foam was brazed with Cu-4.0Sn-9.9Ni-7.8P filler foil for joint strength and interface analysis. Brazed 50 pores per inch (PPI) Cu foam yielded a maximum compressive strength of 14.4 MPa with a 127% increment compared to nonbrazed Cu foam. 15 PPI Cu foam produced a maximum shear strengt...