Effects of post- oxidation annealing temperature on ZrO2 thin film deposited on 4H-SiC substrate

ZrO2 thin film has been formed on n-type 4H-SiC substrate using a combination of metal sputtering (∼25 nm thick) and thermal oxidation (15 min at 500 °C) processes. Effects of post-oxidation annealing temperature (600–900 °C) on the physical and electrical properties of the thin film have been inves...