Effect of high temperature corrosion on austenitic stainless steel grade 304 in CO2 gas at 700ºC
Austenitic stainless steels of grade 304 were exposed to dry (Ar-75%CO2) and wet (Ar-75%CO2-12%H2O) environments at 700oC. This experimental setup involved horizontal tube furnace connected to CO2 gas and water vapour facilities. X-ray diffraction (XRD) technique, variable pressure-scanning electron...
Saved in:
Main Authors: | Nurul Atikah Shariff,, Azman Jalar,, Muhamad Izhar Sahri,, Norinsan Kamil Othman, |
---|---|
Format: | Article |
Language: | English |
Published: |
Universiti Kebangsaan Malaysia
2014
|
Online Access: | http://journalarticle.ukm.my/7263/1/14_Nurul_Atikah.pdf http://journalarticle.ukm.my/7263/ http://www.ukm.my/jsm/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
CHARACTERIZATION AND HOT CORROSION BEHAVIOR OF BOILER TUBE STEELS AT 700oC
by: ENGONGA OBONO, LILIOSA-EYANG
Published: (2014) -
CHLORIDE STRESS CORROSION CRACKING FOR 304L AUSTENITIC STAINLESS STEEL
by: TAJUL ARIFFIN, MOHD ARIF
Published: (2017) -
Study of Spot Welding of Austenitic Stainless Steel Type 304
by: Shamsul Baharin Jamaludin, Assoc. Prof. Dr., et al.
Published: (2008) -
Corrosion Mechanism Study on Welded Austenitic Stainless Steel
by: Ahmad Rahim, Farhana Aqilah
Published: (2018) -
Carbon diffusion in 304I austenitic stainless steel at 650 steel at 650 -750°c in carburizing environment
by: Mohamed Haider, Farag I., et al.