High temperature corrosion behaviour of austenitic stainless steel with CaCO₃ and MgCO₃ deposit

The high temperature corrosion behaviour of austenitic stainless steel was studied at 850°C, 900°C, 950°C and 1000°C for 24 to 120 hr exposure time with CaCO₃ and MgCO₃ deposit. Two commercial available austenitic stainless steel grade of AISI 304 and AISI 316L were selected. Austenitic stainless...