Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism

The development of low thermal mass cement-sand block by incorporating peat soil and Effective Microorganism (EM) was studied systematically. In total, seven mixtures of cement-sand block targeted at a 28-days compressive strength of 7 MPa are designed. One control sample is made with a water/cement...

Full description

Saved in:
Bibliographic Details
Main Authors: Idris, I.H.M., Yusof, N.Z.
Format: Article
Published: Elsevier Ltd 2018
Online Access:https://www.scopus.com/inward/record.uri?eid=2-s2.0-85034736308&doi=10.1016%2fj.cscm.2017.11.004&partnerID=40&md5=505608df1375aa9dce3d48fc023ad148
http://eprints.utp.edu.my/21511/
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.utp.eprints.21511
record_format eprints
spelling my.utp.eprints.215112018-08-01T03:15:52Z Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism Idris, I.H.M. Yusof, N.Z. The development of low thermal mass cement-sand block by incorporating peat soil and Effective Microorganism (EM) was studied systematically. In total, seven mixtures of cement-sand block targeted at a 28-days compressive strength of 7 MPa are designed. One control sample is made with a water/cement ratio (w/c) of 0.5, three mixes using 3, 6 and 10 peat soil replacing sand and three mixes using 10, 20 and 30 EM replacing water. Modified blocks with 6 of peat soil and 30 of EM are the most optimum blocks to be used in the construction of masonry as they successfully reduced the thermal conductivity of the blocks with the value of 1.275 W/mK and 1.792 W/mK respectively when being compared to the thermal conductivity of the control sample which is 2.400 W/mK. Besides, they are also able to achieve higher strength than the desired compressive strength which is 7 MPa. The compressive strength of the samples with 6 of peat soil is 16.48 MPa at 28-days while 30.39 MPa for samples with 30 of EM. On the other hand, the water absorption rate of samples with 6 of peat soil is 7.6 while 6.1 for samples with 30 EM and both are okay since their rate of water absorption is lower than 20. In conclusion, the addition of peat soil and EM in the cement-sand mix show promising performance as a low cost material to produce low thermal mass cement-sand block. © 2017 The Authors Elsevier Ltd 2018 Article NonPeerReviewed https://www.scopus.com/inward/record.uri?eid=2-s2.0-85034736308&doi=10.1016%2fj.cscm.2017.11.004&partnerID=40&md5=505608df1375aa9dce3d48fc023ad148 Idris, I.H.M. and Yusof, N.Z. (2018) Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism. Case Studies in Construction Materials, 8 . pp. 8-15. http://eprints.utp.edu.my/21511/
institution Universiti Teknologi Petronas
building UTP Resource Centre
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Teknologi Petronas
content_source UTP Institutional Repository
url_provider http://eprints.utp.edu.my/
description The development of low thermal mass cement-sand block by incorporating peat soil and Effective Microorganism (EM) was studied systematically. In total, seven mixtures of cement-sand block targeted at a 28-days compressive strength of 7 MPa are designed. One control sample is made with a water/cement ratio (w/c) of 0.5, three mixes using 3, 6 and 10 peat soil replacing sand and three mixes using 10, 20 and 30 EM replacing water. Modified blocks with 6 of peat soil and 30 of EM are the most optimum blocks to be used in the construction of masonry as they successfully reduced the thermal conductivity of the blocks with the value of 1.275 W/mK and 1.792 W/mK respectively when being compared to the thermal conductivity of the control sample which is 2.400 W/mK. Besides, they are also able to achieve higher strength than the desired compressive strength which is 7 MPa. The compressive strength of the samples with 6 of peat soil is 16.48 MPa at 28-days while 30.39 MPa for samples with 30 of EM. On the other hand, the water absorption rate of samples with 6 of peat soil is 7.6 while 6.1 for samples with 30 EM and both are okay since their rate of water absorption is lower than 20. In conclusion, the addition of peat soil and EM in the cement-sand mix show promising performance as a low cost material to produce low thermal mass cement-sand block. © 2017 The Authors
format Article
author Idris, I.H.M.
Yusof, N.Z.
spellingShingle Idris, I.H.M.
Yusof, N.Z.
Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
author_facet Idris, I.H.M.
Yusof, N.Z.
author_sort Idris, I.H.M.
title Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
title_short Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
title_full Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
title_fullStr Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
title_full_unstemmed Development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
title_sort development of low thermal mass cement-sand block utilizing peat soil and effective microorganism
publisher Elsevier Ltd
publishDate 2018
url https://www.scopus.com/inward/record.uri?eid=2-s2.0-85034736308&doi=10.1016%2fj.cscm.2017.11.004&partnerID=40&md5=505608df1375aa9dce3d48fc023ad148
http://eprints.utp.edu.my/21511/
_version_ 1738656299790368768
score 13.211869