Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating

This study presents the influences of talc as an additive in intumescent coating formulations on the thermal insulation, degradation and water resistance. The fire test was performed according to ASTM-E119 standard to study the heat shielding properties of the coated substrates. The results showed t...

Full description

Saved in:
Bibliographic Details
Main Authors: Hazwani Dzulkafli, H., Ahmad, F., Ullah, S., Hussain, P., Mamat, O., Megat-Yusoff, P.S.M.
Format: Article
Published: Elsevier Ltd 2017
Online Access:https://www.scopus.com/inward/record.uri?eid=2-s2.0-85021260704&doi=10.1016%2fj.clay.2017.06.013&partnerID=40&md5=bd06603d253aff79f91b83efc2f0e952
http://eprints.utp.edu.my/19359/
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.utp.eprints.19359
record_format eprints
spelling my.utp.eprints.193592018-04-20T00:21:57Z Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating Hazwani Dzulkafli, H. Ahmad, F. Ullah, S. Hussain, P. Mamat, O. Megat-Yusoff, P.S.M. This study presents the influences of talc as an additive in intumescent coating formulations on the thermal insulation, degradation and water resistance. The fire test was performed according to ASTM-E119 standard to study the heat shielding properties of the coated substrates. The results showed that the 20 of the talc enhanced the heat shielding and recorded substrate temperature 75 °C after 100 min of fire test. The morphology of the char was analyzed by Scanning Electron Microscopy (SEM). X-ray fluorescence (XRF), X-ray Diffraction (XRD) and Fourier Transform Infrared Spectroscopy (FTIR) results showed the presence of P2O5, MgO, TiO2, and SiO2 respectively. The functional groups analysis of char confirmed the presence of high temperature compounds and enhanced thermal performance of coatings. Thermogravimetric analysis (TGA) showed that addition of 20 talc increased residual mass of the char by 55.55. The lap shear test result showed that the talc also improved the adhesion of the intumescent coating with steel substrate and the highest shear strength observed was 7 MPa for a formulation, F5 containing 20 talc. Water immersion test was performed according to ASTM D870-15 and the results showed the higher water-resistance was recorded for a formulation containing 10 talc in the control formulation. © 2017 Elsevier B.V. Elsevier Ltd 2017 Article PeerReviewed https://www.scopus.com/inward/record.uri?eid=2-s2.0-85021260704&doi=10.1016%2fj.clay.2017.06.013&partnerID=40&md5=bd06603d253aff79f91b83efc2f0e952 Hazwani Dzulkafli, H. and Ahmad, F. and Ullah, S. and Hussain, P. and Mamat, O. and Megat-Yusoff, P.S.M. (2017) Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating. Applied Clay Science, 146 . pp. 350-361. http://eprints.utp.edu.my/19359/
institution Universiti Teknologi Petronas
building UTP Resource Centre
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Teknologi Petronas
content_source UTP Institutional Repository
url_provider http://eprints.utp.edu.my/
description This study presents the influences of talc as an additive in intumescent coating formulations on the thermal insulation, degradation and water resistance. The fire test was performed according to ASTM-E119 standard to study the heat shielding properties of the coated substrates. The results showed that the 20 of the talc enhanced the heat shielding and recorded substrate temperature 75 °C after 100 min of fire test. The morphology of the char was analyzed by Scanning Electron Microscopy (SEM). X-ray fluorescence (XRF), X-ray Diffraction (XRD) and Fourier Transform Infrared Spectroscopy (FTIR) results showed the presence of P2O5, MgO, TiO2, and SiO2 respectively. The functional groups analysis of char confirmed the presence of high temperature compounds and enhanced thermal performance of coatings. Thermogravimetric analysis (TGA) showed that addition of 20 talc increased residual mass of the char by 55.55. The lap shear test result showed that the talc also improved the adhesion of the intumescent coating with steel substrate and the highest shear strength observed was 7 MPa for a formulation, F5 containing 20 talc. Water immersion test was performed according to ASTM D870-15 and the results showed the higher water-resistance was recorded for a formulation containing 10 talc in the control formulation. © 2017 Elsevier B.V.
format Article
author Hazwani Dzulkafli, H.
Ahmad, F.
Ullah, S.
Hussain, P.
Mamat, O.
Megat-Yusoff, P.S.M.
spellingShingle Hazwani Dzulkafli, H.
Ahmad, F.
Ullah, S.
Hussain, P.
Mamat, O.
Megat-Yusoff, P.S.M.
Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
author_facet Hazwani Dzulkafli, H.
Ahmad, F.
Ullah, S.
Hussain, P.
Mamat, O.
Megat-Yusoff, P.S.M.
author_sort Hazwani Dzulkafli, H.
title Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
title_short Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
title_full Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
title_fullStr Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
title_full_unstemmed Effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
title_sort effects of talc on fire retarding, thermal degradation and water resistance of intumescent coating
publisher Elsevier Ltd
publishDate 2017
url https://www.scopus.com/inward/record.uri?eid=2-s2.0-85021260704&doi=10.1016%2fj.clay.2017.06.013&partnerID=40&md5=bd06603d253aff79f91b83efc2f0e952
http://eprints.utp.edu.my/19359/
_version_ 1738656058941898752
score 13.211869