High temperature creep behavior of austenitic fe-ni-cr alloy
reep damage investigation was carried out in Fe-Ni-Cr alloy at 800°C, 900°C, and 983°C using rectangular section form of specimen. In all the tests conducted on this material, some creep curves showed primary stage, secondary stage and tertiary stage. The creep fracture shows ductile transgranular f...