Effects of lanthanum strontium cobalt ferrite (LSCF) cathode properties on hollow fibre micro-tubular SOFC performances

Single layer La0.6Sr0.4Co0.2Fe0.8O3 hollow fibre (HF) precursors (<1 mm ID) produced by phase inversion (PI) were sintered at 1,200, 1,350 and 1,400 °C. The increase in sintering temperature resulted in microstructural changes in the LSCF fibres, reflected in their electrical conductivities. LSCF...