Effect of temperature and calcination time in the characterizations of MCM-41
The mesoporous silica particle, MCM-41 has received much attention because of its ease to synthesize and its vast applications as adsorbents and in catalytic reactions. The temperature used was changed from 28°C to 100°C during the synthesis of MCM-41 and it was found that the dissolution time is de...