Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process
A method of solid-state recycling aluminum alloy using hot press forging process was studied as well as the possibility of the recycled chip to be used as secondary resources. This paper presents the results of recycled AA6061 aluminium alloy chip using different operating temperature for hot press...
Saved in:
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Trans Tech Publications
2014
|
Subjects: | |
Online Access: | http://eprints.uthm.edu.my/3962/1/AJ%202017%20%28548%29.pdf http://eprints.uthm.edu.my/3962/ https://dx.doi.org/10.4028/www.scientific.net/AMM.315.728 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.uthm.eprints.3962 |
---|---|
record_format |
eprints |
spelling |
my.uthm.eprints.39622021-11-22T07:55:30Z http://eprints.uthm.edu.my/3962/ Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process Yusuf, Nur Kamilah Lajis, Mohd Amri Daud, M.I. Noh, Mohamad Zaky TA401-492 Materials of engineering and construction. Mechanics of materials A method of solid-state recycling aluminum alloy using hot press forging process was studied as well as the possibility of the recycled chip to be used as secondary resources. This paper presents the results of recycled AA6061 aluminium alloy chip using different operating temperature for hot press forging process. Mechanical properties and microstructure of the recycled specimens and as-received (reference) specimen were investigated. The recycled specimens exhibit a good potential in the strength properties. The result for yield strength (YS) and ultimate tensile strength (UTS) at the minimum temperature 430˚C is 25.8 MPa and 27.13 MPa. For the maximum operating temperature 520˚C YS and UTS are 107.0MPa and 117.53 MPa. Analysis for different operating temperatures shows that the higher temperatures giving better result on mechanical properties and finer microstructure. The strength of recycled specimen increases due to the grain refinement strengthening whereas particle dispersion strengthening has minor effects. In this study, the recycled AA6061 chip shows the good potential in strengthening as the comparison of using only 17.5% of suggested pressure (70.0/400.0) MPa, the UTS exhibit 35.8% (117.58/327.69) MPa. This shows a remarkable potential of direct recycling by using hot press forging process. Trans Tech Publications 2014 Article PeerReviewed text en http://eprints.uthm.edu.my/3962/1/AJ%202017%20%28548%29.pdf Yusuf, Nur Kamilah and Lajis, Mohd Amri and Daud, M.I. and Noh, Mohamad Zaky (2014) Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process. Advanced Materials Research, 315 (NIL). pp. 728-732. ISSN 1022-6680 https://dx.doi.org/10.4028/www.scientific.net/AMM.315.728 |
institution |
Universiti Tun Hussein Onn Malaysia |
building |
UTHM Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Tun Hussein Onn Malaysia |
content_source |
UTHM Institutional Repository |
url_provider |
http://eprints.uthm.edu.my/ |
language |
English |
topic |
TA401-492 Materials of engineering and construction. Mechanics of materials |
spellingShingle |
TA401-492 Materials of engineering and construction. Mechanics of materials Yusuf, Nur Kamilah Lajis, Mohd Amri Daud, M.I. Noh, Mohamad Zaky Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process |
description |
A method of solid-state recycling aluminum alloy using hot press forging process was studied as well as the possibility of the recycled chip to be used as secondary resources. This paper presents the results of recycled AA6061 aluminium alloy chip using different operating temperature for hot press forging process. Mechanical properties and microstructure of the recycled specimens and as-received (reference) specimen were investigated. The recycled specimens exhibit a good potential in the strength properties. The result for yield strength (YS) and ultimate tensile strength (UTS) at the minimum temperature 430˚C is 25.8 MPa and 27.13 MPa. For the maximum operating temperature 520˚C YS and UTS are 107.0MPa and 117.53 MPa. Analysis for different operating temperatures shows that the higher temperatures giving better result on mechanical properties and finer microstructure. The strength of recycled specimen increases due to the grain refinement strengthening whereas particle dispersion strengthening has minor effects. In this study, the recycled AA6061 chip shows the good potential in strengthening as the comparison of using only 17.5% of suggested pressure (70.0/400.0) MPa, the UTS exhibit 35.8% (117.58/327.69) MPa. This shows a remarkable potential of direct recycling by using hot press forging process. |
format |
Article |
author |
Yusuf, Nur Kamilah Lajis, Mohd Amri Daud, M.I. Noh, Mohamad Zaky |
author_facet |
Yusuf, Nur Kamilah Lajis, Mohd Amri Daud, M.I. Noh, Mohamad Zaky |
author_sort |
Yusuf, Nur Kamilah |
title |
Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process |
title_short |
Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process |
title_full |
Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process |
title_fullStr |
Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process |
title_full_unstemmed |
Effect of operating temperature on direct recycling aluminium chips (AA6061) in hot press forging process |
title_sort |
effect of operating temperature on direct recycling aluminium chips (aa6061) in hot press forging process |
publisher |
Trans Tech Publications |
publishDate |
2014 |
url |
http://eprints.uthm.edu.my/3962/1/AJ%202017%20%28548%29.pdf http://eprints.uthm.edu.my/3962/ https://dx.doi.org/10.4028/www.scientific.net/AMM.315.728 |
_version_ |
1738581188515201024 |
score |
13.250246 |