Shape Memory Polyurethane Based On Palm Oil Polyol

In this study, shape memory polyurethane (SMPU) was prepared based on palm oil polyol (POP) to reduce the usage of petrochemical based polyol. The amount of POP used was up to 20% and the total reaction time for prepolymer preparation was 2.5 to 5 hours. POP based SMPU was prepared via two-step p...

Full description

Saved in:
Bibliographic Details
Main Author: Rashid, Tuan Nur Izzah Tuan Ab
Format: Monograph
Language:English
Published: Universiti Sains Malaysia 2015
Subjects:
Online Access:http://eprints.usm.my/52865/1/Shape%20Memory%20Polyurethane%20Based%20On%20Palm%20Oil%20Polyol_Tuan%20Nur%20Izzah%20Tuan%20Ab%20Rashid_B1_2015.pdf