Impedance studies on Ca0.5Sr0.5Cu3Ti4O12 ceramic oxide

Ca0.5Sr0.5Cu3Ti4O12 (CSCTO) ceramic oxide was prepared using solid state reaction technique. Impedance measurement was done using High Dielectric Resolution Analyzer (Novocontrol Novotherm) from 30°C to 250°C, in the frequency range of 10-2 to 106 Hz. X-ray diffraction pattern showed a single phase...