A way to limit the long-term degradation of solid oxide fuel cell cathode by decorating the surface with K2NiF4-Structure Pr4Ni3O10+� phase
Prolonged annealing of La0.6Sr0.4Co0.2Fe0.8O3-� (LSCF) at 700 �C for 1000 h resulted in phase segregation on the surface in the form of submicron-sized SrO on the grains and micron-sized CoFe2O4 particles near the grain boundaries during electrical conductivity relaxation (ECR) measurements. The pre...
Saved in:
Main Authors: | Saher S., Tan C.Y., Ramesh S., Yap B.K., Ong B.H., Mo K.H., Al-Furjan M.S.H. |
---|---|
Other Authors: | 36134688200 |
Format: | Article |
Published: |
Elsevier B.V.
2025
|
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Unveiling the role of K2NiF4-Structure Pr4Ni3O10+� surface coverage in boosting oxygen permeation and suppressing membrane degradation
by: Saher S., et al.
Published: (2025) -
Enhancing oxygen exchange kinetics of solid oxide fuel cell cathode: Unleashing the potential of higher order Ruddlesden-Popper phase surface modification
by: Saher S., et al.
Published: (2024) -
Solid electrolyte for intermediate temperature solid Oxide fuel cell
by: Nurul Fatihah, Ahamad
Published: (2022) -
Structure and properties of cathode and electrolyte for intermediate temperature solid oxide fuel cells (IT-SOFCS)
by: Nurhamidah, Zakaria
Published: (2017) -
Characteristic and challenges of scandia stabilized zirconia as solid oxide fuel cell material � In depth review
by: Arifin N.A., et al.
Published: (2024)