Failure analysis on a primary superheater tube of a power plant
In this paper failure analysis on the SA213-T12 superheater tube by visual inspection, in situ measurements of hardness and finite element analyses is presented. A primary superheater tube has failed with a wide open burst after running at around 28,194 h. Heavy clinkers were found to almost entirel...
Saved in:
Main Authors: | Purbolaksono J., Ahmad J., Beng L.C., Rashid A.Z., Khinani A., Ali A.A. |
---|---|
其他作者: | 8621252500 |
格式: | Article |
出版: |
2023
|
主题: | |
标签: |
添加标签
没有标签, 成为第一个标记此记录!
|
相似书籍
-
Root cause failure analysis of a division wall superheater tube of a coal-fired power station
由: Rahman M.M., et al.
出版: (2023) -
Failure evaluation on a high-strength alloy SA213-T91 super heater tube of a power generation
由: Ahmad J., et al.
出版: (2023) -
Failure investigation of a primary superheater tube
由: Rahman M.M., et al.
出版: (2023) -
Failure investigation on deformed superheater tubes
由: Othman H., et al.
出版: (2023) -
Failure analysis on high temperature superheater Inconel� 800 tube
由: Ahmad J., et al.
出版: (2023)