Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature

This thesis mainly presents the investigation of the characteristics of iron powder ASC 100.29 mixed with aluminium (A1) powder formed at room temperature and above room temperature. The iron powder ASC 100.29 was mixed with different weightage of aluminium powder which is 0%, 5%, 10% and 15% compac...

詳細記述

保存先:
書誌詳細
第一著者: Sasikumar A/L Suriya Sandran
フォーマット: text::Thesis
言語:English
出版事項: 2023
主題:
タグ: タグ追加
タグなし, このレコードへの初めてのタグを付けませんか!
id my.uniten.dspace-20969
record_format dspace
spelling my.uniten.dspace-209692023-05-05T04:34:10Z Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature Sasikumar A/L Suriya Sandran Powders This thesis mainly presents the investigation of the characteristics of iron powder ASC 100.29 mixed with aluminium (A1) powder formed at room temperature and above room temperature. The iron powder ASC 100.29 was mixed with different weightage of aluminium powder which is 0%, 5%, 10% and 15% compacted i.e. temperature 30C, 60C, and 90C respectively. Once the compaction process was done, the product of the compaction process is called green sample. There were total 12 green samples generated during the compaction process. 2023-05-03T15:40:32Z 2023-05-03T15:40:32Z 2018 Resource Types::text::Thesis https://irepository.uniten.edu.my/handle/123456789/20969 en application/pdf
institution Universiti Tenaga Nasional
building UNITEN Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Tenaga Nasional
content_source UNITEN Institutional Repository
url_provider http://dspace.uniten.edu.my/
language English
topic Powders
spellingShingle Powders
Sasikumar A/L Suriya Sandran
Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature
description This thesis mainly presents the investigation of the characteristics of iron powder ASC 100.29 mixed with aluminium (A1) powder formed at room temperature and above room temperature. The iron powder ASC 100.29 was mixed with different weightage of aluminium powder which is 0%, 5%, 10% and 15% compacted i.e. temperature 30C, 60C, and 90C respectively. Once the compaction process was done, the product of the compaction process is called green sample. There were total 12 green samples generated during the compaction process.
format Resource Types::text::Thesis
author Sasikumar A/L Suriya Sandran
author_facet Sasikumar A/L Suriya Sandran
author_sort Sasikumar A/L Suriya Sandran
title Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature
title_short Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature
title_full Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature
title_fullStr Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature
title_full_unstemmed Characteristics of iron powder ASC100.29 mixed with aluminium (AL) powder formed at room temperature and above room temperature
title_sort characteristics of iron powder asc100.29 mixed with aluminium (al) powder formed at room temperature and above room temperature
publishDate 2023
_version_ 1806427542909878272
score 13.250246