Preventing delayed cracks in deep drawing processes of SUS304 cylindrical cups using a coated die / Phoo Yoong Hau
Longitudinal delayed cracks tend to form along the sidewall of fully drawn SUS304 metastable austenitic stainless steel cylindrical cups immediately after the deep drawing process for a certain incubation period ranging from several minutes to several days. Although the delayed cracks were eliminate...
Saved in:
Main Author: | Phoo, Yoong Hau |
---|---|
Format: | Thesis |
Published: |
2019
|
Subjects: | |
Online Access: | http://studentsrepo.um.edu.my/11488/1/Phoo_Yoong_Hau.jpg http://studentsrepo.um.edu.my/11488/8/phoo.pdf http://studentsrepo.um.edu.my/11488/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
FE simulation study of deep drawing process of SUS304 cups having no delayed cracks under enhanced blank holding force
by: Tan, Chin Joo, et al.
Published: (2020) -
Preventing delayed cracks in SUS304 deep drawn cups using extreme blank holding forces aided by nanolubrication
by: Tan, Chin Joo, et al.
Published: (2019) -
Study of delayed cracking behaviors of hydrogen-charged SUS304L deep drawn cylindrical cups under elevated blank holding forces / Mohd Shahir Hadzir
by: Mohd Shahir, Hadzir
Published: (2022) -
Preventing delayed cracks in SUS304 deep drawn cups using extreme blank holding forces aided by nanolubrication / Muhammad Shafiq Ibrahim
by: Muhammad Shafiq, Ibrahim
Published: (2020) -
Analysis and experiment of blank holder gap in the cylindrical cup deep drawing of low carbon steel to prevent cracking-wrinkling / Susila Candra and Hudiyo Firmanto
by: Candra, Susila, et al.
Published: (2024)