Lanthanum–titanium oxide composite from a single molecular cluster: Non-enzymatic mesoporous electrochemical nitrite ion sensor

In the present investigation, lanthanum–titanium [La3Ti6O4(OH)6(C2F3O2)13(H2O)2(C4H8O)6] (1) was successfully used as single source precursor to fabricate electrodes of LTO 600 (La4Ti9O24-La2O3-LaTiO3-TiO2(rutile)) and LTO 700 (La4Ti9O24-La2O3) at sintering temperature of 600 and 700 °C, respectivel...

Full description