Brazing of inconel 600 by active filler metal
Inconel 600 alloy was brazed at three (3) different brazing temperatures, 830, 865 and 900°C for 30 minutes. An active filler metal, Ag-Cu- Ti, was utilized to study its effects on bonding strength by the diffusion of some elements with lnconel 600 during brazing. The experiment was carried out in...