The dielectric constant (ɛr =ɛ'r - jɛ"r) and loss tangent (tan δ = ɛ"/ɛ') of different thicknesses of 70% thermoplastic natural rubber-30% yttrium iron garnet (Y3FesO12) composite / Noor Azleen Azmi

Thermoplastic natural rubber (TPNR) was prepared by melt-blending of polypropylene (PP) and natural rubber (NR) in weight percentage ratio of 70:30 using internal Rheomixer. Sample of Yttrium Iron Garnet (Y3FesOI2) filled TPNR was prepared at a fixed TPNR content (70% of the total weight). The ef...