Formation of protective Cr2O3 scale at high temperature and the effect of mass transport in the presence of water vapor
The formation of protective Cr2O3 scale at high temperature was evaluated using Wagner’s theory of binary alloy oxidation. The results show that at 1073 K, around 9.8 wt% of Cr is required to form external Cr2O3 scale, and 3.5wt% of Cr is needed to maintain the scale. Introduction of water vapor has...
Saved in:
Main Authors: | Ani, Mohd Hanafi, Othman, Raihan |
---|---|
Format: | Article |
Language: | English |
Published: |
Trans Tech Publications Ltd., Switzerland
2012
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/16691/1/Formation_of_protective_Cr2O3_scale_at_high_temperature.pdf http://irep.iium.edu.my/16691/ http://www.scientific.net/AMR.402.412 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Observation on void formed in oxide scale of Fe-Cr-Ni alloy at 1073K in dry and humid environments
by: Kaderi, Akbar, et al.
Published: (2011) -
Effect Of High Temperature On Oxidation Behavior Of Superheater Materials Formation Of Protective Oxide Scale
by: Abdul Wahab, Haziq Mudzakir
Published: (2018) -
Surface Oxidation Of CU Extracted From Electronic Waste For CUO Nanowires Formation And Their Use To Reduce CR(VI)
by: Yong, Hui Sin
Published: (2022) -
Microstructural evaluation and corrosion behaviour of Fe-Cr-Ni-Mn-Co AND AI0.5-Fe-Cr-Ni-Mn-Co highentropy alloys (HEA) with elemental additions / Siti Sarah Mohd Pauzi
by: Mohd Pauzi, Siti Sarah
Published: (2018) -
Studies on initial stage of high temperature oxidation of Fe - 9 to 12% Cr alloys in water vapour environment
by: Kaderi, Akbar, et al.
Published: (2012)