Electrical properties and microstructure of magnetoresistive ( (x = 0.0, 0.05, 0.15 and 0.3)
The insulator-metal transition temperature, Tim of (x = 0.0, 0.05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain s...
Saved in:
Main Authors: | , , |
---|---|
Format: | Article |
Published: |
Universiti Kebangsaan Malaysia
2006
|
Online Access: | http://journalarticle.ukm.my/3993/ http://www.ukm.my/jsm/english_journals/vol35num2_2006/vol35num2_06page73-77.html |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my-ukm.journal.3993 |
---|---|
record_format |
eprints |
spelling |
my-ukm.journal.39932012-05-07T04:33:46Z http://journalarticle.ukm.my/3993/ Electrical properties and microstructure of magnetoresistive ( (x = 0.0, 0.05, 0.15 and 0.3) Ewe, L.S. Hamid, N.A. Abd-Shukor, R. The insulator-metal transition temperature, Tim of (x = 0.0, 0.05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain size is in the range of 0.6 µm - 1.4 µm. Grain boundaries are almost completely revealed for x = 0.3. X-Ray powder diffraction patterns showed cubic structure (space group Pm-3m) and contain no secondary phases. Universiti Kebangsaan Malaysia 2006-12 Article PeerReviewed Ewe, L.S. and Hamid, N.A. and Abd-Shukor, R. (2006) Electrical properties and microstructure of magnetoresistive ( (x = 0.0, 0.05, 0.15 and 0.3). Sains Malaysiana, 35 (2). pp. 73-77. ISSN 0126-6039 http://www.ukm.my/jsm/english_journals/vol35num2_2006/vol35num2_06page73-77.html |
institution |
Universiti Kebangsaan Malaysia |
building |
Perpustakaan Tun Sri Lanang Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Kebangsaan Malaysia |
content_source |
UKM Journal Article Repository |
url_provider |
http://journalarticle.ukm.my/ |
description |
The insulator-metal transition temperature, Tim of (x = 0.0, 0.05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain size is in the range of 0.6 µm - 1.4 µm. Grain boundaries are almost completely revealed for x = 0.3. X-Ray powder diffraction patterns showed cubic structure (space group Pm-3m) and contain no secondary phases. |
format |
Article |
author |
Ewe, L.S. Hamid, N.A. Abd-Shukor, R. |
spellingShingle |
Ewe, L.S. Hamid, N.A. Abd-Shukor, R. Electrical properties and microstructure of magnetoresistive ( (x = 0.0, 0.05, 0.15 and 0.3) |
author_facet |
Ewe, L.S. Hamid, N.A. Abd-Shukor, R. |
author_sort |
Ewe, L.S. |
title |
Electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3) |
title_short |
Electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3) |
title_full |
Electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3) |
title_fullStr |
Electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3) |
title_full_unstemmed |
Electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3) |
title_sort |
electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3) |
publisher |
Universiti Kebangsaan Malaysia |
publishDate |
2006 |
url |
http://journalarticle.ukm.my/3993/ http://www.ukm.my/jsm/english_journals/vol35num2_2006/vol35num2_06page73-77.html |
_version_ |
1643735922482610176 |
score |
13.211869 |