Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials

The objectives of this study were to measure and compare the bond strength between selective orthodontics adhesives and anterior restorative materials. 104 extracted bovine incisors were selected and divided into four groups of 26 each, etched with 37% phosphoric acid, primed with Prime & Bond O...

詳細記述

保存先:
書誌詳細
主要な著者: Muhamad Halil, Mohd Haikal, Zainol, Iswan Zuraidi, Chi Adam, Khairul Bariah, Wan Rosman, Wan Nur Farhana, Ahmad, Siti Zulaikha
フォーマット: 論文
言語:English
English
出版事項: University of Dicle 2019
主題:
オンライン・アクセス:http://irep.iium.edu.my/82169/1/82169_Comparison%20of%20Bond%20Strength.pdf
http://irep.iium.edu.my/82169/2/82169_Comparison%20of%20Bond%20Strength_SCOPUS.pdf
http://irep.iium.edu.my/82169/
http://www.jidmr.com/journal/wp-content/uploads/2019/12/7.19274-ED-A-291019-fl.pdf
タグ: タグ追加
タグなし, このレコードへの初めてのタグを付けませんか!
id my.iium.irep.82169
record_format dspace
spelling my.iium.irep.821692020-08-13T13:43:40Z http://irep.iium.edu.my/82169/ Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials Muhamad Halil, Mohd Haikal Zainol, Iswan Zuraidi Chi Adam, Khairul Bariah Wan Rosman, Wan Nur Farhana Ahmad, Siti Zulaikha RK Dentistry RK318 Oral and Dental Medicine. Pathology. Diseases-Therapeutics-General Works The objectives of this study were to measure and compare the bond strength between selective orthodontics adhesives and anterior restorative materials. 104 extracted bovine incisors were selected and divided into four groups of 26 each, etched with 37% phosphoric acid, primed with Prime & Bond One (Dentsply) and bonded in dry field to enamel surfaces using four different adhesive materials. The materials tested were: Transbond XT(3M), Lightbond(Reliance), Filtek Z350XT(3M) and Neofil (Kerr). These samples then underwent thermal and acidic exposure for two time intervals, at twenty four hours and three months and finally the shear bond strength were measured using Instron Universal Testing machine. The data then analysed using SPSS Compare Means-Paired Sample T-Test. Lightbond (OA) showed the highest mean value of bond strength at both 24 hours and three months' time interval which was 13.95 MPa. This followed by Transbond XT (OA) that exhibit lower value at 9.63 MPa. Filtek Z350 (AR) had the highest bond strength among the anterior restorative materials tested at 9.18 MPa while the Neofil (AR) has shown significantly lower and consistent mean bond strength in both time intervals among all materials which was 7.88 MPa. Orthodontics adhesives have higher bond strength to bovine enamel compared to anterior restorative materials. © 2019 University of Dicle. University of Dicle 2019 Article PeerReviewed application/pdf en http://irep.iium.edu.my/82169/1/82169_Comparison%20of%20Bond%20Strength.pdf application/pdf en http://irep.iium.edu.my/82169/2/82169_Comparison%20of%20Bond%20Strength_SCOPUS.pdf Muhamad Halil, Mohd Haikal and Zainol, Iswan Zuraidi and Chi Adam, Khairul Bariah and Wan Rosman, Wan Nur Farhana and Ahmad, Siti Zulaikha (2019) Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials. Journal of International Dental and Medical Research, 12 (4). pp. 1274-1279. ISSN 1309-100X http://www.jidmr.com/journal/wp-content/uploads/2019/12/7.19274-ED-A-291019-fl.pdf
institution Universiti Islam Antarabangsa Malaysia
building IIUM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider International Islamic University Malaysia
content_source IIUM Repository (IREP)
url_provider http://irep.iium.edu.my/
language English
English
topic RK Dentistry
RK318 Oral and Dental Medicine. Pathology. Diseases-Therapeutics-General Works
spellingShingle RK Dentistry
RK318 Oral and Dental Medicine. Pathology. Diseases-Therapeutics-General Works
Muhamad Halil, Mohd Haikal
Zainol, Iswan Zuraidi
Chi Adam, Khairul Bariah
Wan Rosman, Wan Nur Farhana
Ahmad, Siti Zulaikha
Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
description The objectives of this study were to measure and compare the bond strength between selective orthodontics adhesives and anterior restorative materials. 104 extracted bovine incisors were selected and divided into four groups of 26 each, etched with 37% phosphoric acid, primed with Prime & Bond One (Dentsply) and bonded in dry field to enamel surfaces using four different adhesive materials. The materials tested were: Transbond XT(3M), Lightbond(Reliance), Filtek Z350XT(3M) and Neofil (Kerr). These samples then underwent thermal and acidic exposure for two time intervals, at twenty four hours and three months and finally the shear bond strength were measured using Instron Universal Testing machine. The data then analysed using SPSS Compare Means-Paired Sample T-Test. Lightbond (OA) showed the highest mean value of bond strength at both 24 hours and three months' time interval which was 13.95 MPa. This followed by Transbond XT (OA) that exhibit lower value at 9.63 MPa. Filtek Z350 (AR) had the highest bond strength among the anterior restorative materials tested at 9.18 MPa while the Neofil (AR) has shown significantly lower and consistent mean bond strength in both time intervals among all materials which was 7.88 MPa. Orthodontics adhesives have higher bond strength to bovine enamel compared to anterior restorative materials. © 2019 University of Dicle.
format Article
author Muhamad Halil, Mohd Haikal
Zainol, Iswan Zuraidi
Chi Adam, Khairul Bariah
Wan Rosman, Wan Nur Farhana
Ahmad, Siti Zulaikha
author_facet Muhamad Halil, Mohd Haikal
Zainol, Iswan Zuraidi
Chi Adam, Khairul Bariah
Wan Rosman, Wan Nur Farhana
Ahmad, Siti Zulaikha
author_sort Muhamad Halil, Mohd Haikal
title Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
title_short Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
title_full Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
title_fullStr Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
title_full_unstemmed Comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
title_sort comparison of bond strength between selected orthodontic adhesives versus anterior restorative materials
publisher University of Dicle
publishDate 2019
url http://irep.iium.edu.my/82169/1/82169_Comparison%20of%20Bond%20Strength.pdf
http://irep.iium.edu.my/82169/2/82169_Comparison%20of%20Bond%20Strength_SCOPUS.pdf
http://irep.iium.edu.my/82169/
http://www.jidmr.com/journal/wp-content/uploads/2019/12/7.19274-ED-A-291019-fl.pdf
_version_ 1675327180622528512
score 13.250246